| 性质/条件 | 单位 | 参考限值 | 测试方法 |
|---|---|---|---|
| Kinematic viscosity at 60°C | mm²/s | 800-1600 | ASTM D2170 |
| Flash point (Cleveland open cup) | °C | ≥70 | ASTM D92 |
| Water content | % | ≤0.5 | ASTM D95 |
| Solubility in trichloroethylene | % | ≥95 | ASTM D2042 |
| DISTILLATION AND RECOVERED RESIDUE | |||
| Total distillate collected to 360°C | vol % | ≤15 | ASTM D402 |
| ASPHALT RESIDUE OF SPECIFIED PENETRATION | |||
| Residue of 100 penetration | % | ≥60 | ASTM D243 |
| Ductility of 100 penetration residue at 25°C | cm | ≥50 | ASTM D113 |